AISI S7

Typical analysis

C
Cr
Mo
0.50
3.25
1.40

Designed for use where the ability to withstand repeated blows at normal operating temperatures is more important than the ability to resist wear and abrasion.

Typical applications

Hand and pneumatic tools for chipping, punching, riveting, as well as drift pins, grippers, mandrels, heavy duty blanking and forming dies and shears blades.

Thermal Treatments Degrees Celsius
Forging 1120°C - 950°C
Annealing

815°C - 840°C Tensile strength as Annealed
( 45 - 52 tons per Sq. inch )
Hardness: 187 - 223 BHN

Hardening 925°C - 950°C

Tempering
( maximum wear )

205°C - 260°C

Tempering
( maximum toughness )
480°C - 540°C
Quenching medium Air ( Section greater than 2 - 1/2" flash
oil quench )
Obtainable hardness
( HRC )
45 - 57
Wear resistance Medium
Toughness Very high
Distortion in heat treating Lowest
Machinability Medium
Red hardness High
 
home
forging
treating
steels
standards
tools
glossary
computers
    others
links
sponsors
site map
about EM
contact EM
 
EM® is property of CAMSteel Ltd.© However you can copy parts of this site with prior notification
1